Description Mortars with lips are glazed on the outside, except for the bottom. Pestles are glazed to grinding surface. Oversized pestle for easier grinding. Features: • Thermal Shock Resistance - Average coefficient of expansion from 20°C to 200°C is 3.56 x 10-5, gradually increasing to 4.69 x 10-5 at 1000°C. Every batch of porcelain is heat tested in our factory.. • Glaze - No softening occurs up to 1000°C, and it is extremely white.. • Resistance to Chemical ... Read more
In Stock!

Starting at from $8.38 Sale $7.54

Description Mortars with lips are glazed on the outside, except for the bottom. Pestles are glazed to grinding surface. Oversized pestle for easier grinding. Features: • Thermal Shock Resistance - Average coefficient of expansion from 20°C to 200°C is 3.56 x 10-5, gradually increasing to 4.69 x 10-5 at 1000°C. Every batch of porcelain is heat tested in our factory.. • Glaze - No softening occurs up to 1000°C, and it is extremely white.. • Resistance to Chemical ... Read more